WCB | 碳钢 | ASTM A216 | 无腐蚀性应用,包括水,油和气,温度范围:-30oC至+425oC |
LCB | 低温碳钢 | ASTM A352 | 低温应用,温度低至-46oC 不能用于温度高于+340oC的场合 |
LC3 | 3.5%镍钢 | ASTM A352 | 低温应用,温度低至-101oC 不能用于温度高于+340oC的场合 |
WC6 | 1.25%铬0.5%钼钢 | ASTM A217 | 无腐蚀性应用,包括水,油和气,温度范围:-30oC至+593oC |
WC9 | 2.25铬 | ASTM A217 | 无腐蚀性应用,包括水,油等级WC9和气,温度范围:-30oC至+593oC |
C5 | 5%铬0.5%钼 | ASTM A217 | 轻度腐蚀性或侵蚀性应用及无腐蚀性应用,温度范围:-30oC至+649oC |
C12 | 9%铬1%钼 | ASTM A217 | 轻度腐蚀性或侵蚀性应用及无腐蚀性应用,温度范围:-30oC至+649oC |
CA6NM(4) | 12%铬钢 | ASTM A487 | 腐蚀性应用,温度范围:-30oC至+482oC |
CA15(4) | 12%铬 | ASTM A217 | 腐蚀性应用, 温度范围高达+704oC |
CF8M 3 | 16不锈钢 | ASTM A351 | 腐蚀性或超低温或高温无腐蚀性应用,温度范围:-268oC至+649oC, |
CF8C | 347不锈钢 | ASTM A351 | 主要用于高温,腐蚀性应用,温度范围:-268oC至+649oC, |
CF8 | 304不锈钢 | ASTM A351 | 腐蚀性或超低温或高温无腐蚀性应用,温度范围:-268oC至+649oC, |
CF3 | 304L不锈钢 | ASTM A351 | 腐蚀性或无腐蚀性应用, 温度范围高达+425oC |
欢迎光临 专业阀门论坛_阀门技术|阀门标准|阀门资料 (http://en.china-acg.com/discuz/) | Powered by Discuz! X2.5 |